ITG-10.1R-18: Report on Alternative Cements

ITG-10.1R-18: Report on Alternative Cements

Your Price: $ 59.50 USD

Member Price: $ 39.00 USD

Save $ 20.50 USD, Become a Member

Choose Product Language

Choose Product Format

Notes/Preview

Preview

Description

This report addresses available and emerging alternative cements with the intent to facilitate the adoption of these new materials. Given the initiatives to address the sustainability of construction, owners, architects, and engineers are actively seeking alternatives to portland cement for concrete. An alternative cement is intended to be a replacement for portland cement in some applications. In some cases, alternative cements can also be used in combination with portland or blended hydraulic cements. In addition to a reduced environmental impact associated with their production and use, alternative cements offer improved performance over portland cement in some applications. Various alternative cement technologies are discussed, including their physical and compositional characteristics, methods of production, fresh and hardened properties, and example applications. Additionally, the applicability of existing tests methods for specifying alternative cements is discussed and new testing needs are identified.

Keywords: alkali-activated; alternative cementitious materials; alternative cements; calcium aluminate cement; calcium sulfoaluminate cement; carbonated calcium silicate cement; geopolymer; magnesium oxychloride cement; magnesium phosphate cement; supersulfated cement.

 

Document Details

Author: ACI Committee 93

Pages: 26.00

ISBN: 9781641950244

Categories: Cementitious Materials

Formats: Printed Document or PDF

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1 —Introduction

1.2—Scope

1.3—History

CHAPTER 2—DEFINITIONS

CHAPTER 3—BACKGROUND

3.1—Performance measures for alternative cements

3.2—Summary

CHAPTER 4—ALTERNATIVE CEMENT TECHNOLOGIES

4.1—Introduction

4.2—Clinkered alternative cements

4.3—Calcined alternative cements

4.4—Non-clinkered alternative cements

4.5—Summary

CHAPTER 5—TESTING REQUIREMENTS FOR ALTERNATIVE CEMENT TECHNOLOGIES

5.1—Introduction

5.2—Testing alternative cements

5.3—Testing alternative cement concrete

5.4—Summary

CHAPTER 6—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).