Table of Contents
Learning Objectives
1. Explain the process by which galvanic technology protects the reinforcement in concrete;
2. Discuss suitable repair materials that can be used;
3. Recognize the impact of steel density on the spacing of anodes; and
4. Describe proper anode placement.