503.2-92 (Reapproved 2003)

This specification describes the work of bonding plastic concrete to hardened concrete with a multi-component epoxy adhesive such as defined speci-for this purpose in ASTM C 881. It includes controls for adhesive labeling, supple-storage, handling, mixing and application, surface evaluation and pre-paration as well as inspection and quality control.

Keywords: adhesives; bond (concrete to concrete); bonding; concrete construction; epoxy resins; fresh concretes; hardened concrete; quality control; repairs; specifications; standards

503.3-10

This specification describes the work of producing a skid-resistant surface on hardened concrete by the application of a multi-component epoxy resin. It includes controls for resin labeling, storage, handling, mixing, and application; surface evaluation and preparation; and inspection and quality. In addition, it describes an aggregate to be used with the coating.

Keywords: aggregates; coatings; concrete pavements; epoxy resins; hardened concrete; quality control; skid resistance; specification; standards

503.4-92 (Reapproved 2003):

This specification describes the work of repairing defects in hardened portland cement concrete with a sand-filled mortar using an adhesive binder such as defined in ASTM C 881. It includes controls for adhesive labeling storage, handling, mixing and application, surface evaluation and preparation as well as inspection and quality control.

Keywords: bond (concrete to concrete); concrete construction; epoxy resins, hardened concrete; mortars (material); quality control; repairs; resurfacing; specifications; standards.

Document Details

Author: ACI Committee 503

Publication Year: 2017

Pages: 0

ISBN:

Categories: Epoxies

Formats: PDF

Table of Contents

This publication includes the following documents:

503.2-92 (Reapproved 2003): Standard Specifications for Bonding Plastic Concrete to hardened Concrete with a Multi-Component Epoxy Adhesive.

503.3-10: Specification for Producing a Skid-Resistant Surface on Concrete by the Use of Epoxy and Aggregate.

503.4-92 (Reapproved 2003): Standard Specifications for Repairing Concrete with Epoxy Mortars.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the Manual of Concrete Practice (MCP). For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).