439.4R-09 Report on Steel Reinforcement - Material Properties and U.S. Availability (Reapproved 2017)

439.4R-09 Report on Steel Reinforcement - Material Properties and U.S. Availability (Reapproved 2017)

Your Price: $ 53.50 USD

Member Price: $ 32.00 USD

Save $ 21.50 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

Preview

Description

The material properties of the various types of steel reinforcement produced for use in the United States are described. Types of steel reinforcement defined in this report include deformed reinforcing bars, plain and deformed wire, welded wire reinforcement, bar mats, and prestressing reinforcement. The requirements, restrictions, and testing information of the pertinent ASTM specifications are reviewed. The availability of the various types and sizes of reinforcement in the U. S. is discussed.

Keywords: bend tests; bending (reinforcing steels); deformed reinforcement; deformed reinforcing bars; ductility; material properties; prestressing steels; reinforced concrete; reinforcing steels; specifications; spiral reinforcement; tensile strength; welded reinforcement grids; welded wire fabric; welded wire reinforcement; yield strength.

 

Document Details

Author: ACI Committee 439

Publication Year: 2009

Pages: 19.00

ISBN: 9780870313486

Categories: Reinforcement

Formats: PDF

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Reinforcing bars

3.1—Introduction

3.2—Material properties

3.3—Availability

3.4—Welding

3.5—Material testing

3.6—Spirals and mats

3.7—Corrosion protection products

Chapter 4—Plain and deformed wire

4.1—Introduction

4.2—Material properties

4.3—Wire size designation

4.4—Availability

4.5—Corrosion protection products

Chapter 5—Welded wire reinforcement

5.1—Introduction

5.2—Material properties

5.3—Higher-strength welded wire reinforcement

5.4—Welded wire reinforcement styles

5.5—Availability

5.6—Minimum quantity requirements

5.7—Corrosion protection products

Chapter 6—Prestressing reinforcement

6.1—Introduction

6.2—Material properties

6.3—Availability

6.4—Corrosion protection products

6.5—Other prestressing reinforcement

Chapter 7—Developments in reinforcing steel

7.1—High relative rib area reinforcing bars

7.2—Low-carbon, chromium steel reinforcing bars

Chapter 8—References

8.1—Referenced standards and reports

8.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).