437.2M-13 Code Requirements for Load Testing of Existing Concrete Structures and Commentary (Metric)

437.2M-13 Code Requirements for Load Testing of Existing Concrete Structures and Commentary (Metric)

Currency Display

Your Price: $ 65.50 USD

Member Price: $ 42.00 USD

Save $ 23.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Notes/Preview

Preview

Description

This code provides requirements for test load magnitudes, test protocols, and acceptance criteria for conducting a load test as a means of evaluating the safety and serviceability of concrete structural members and systems for existing buildings as provided for by ACI 562-13. A load test may be conducted as part of a structural evaluation to determine whether an existing building requires

repair and rehabilitation, or to verify the adequacy of repair and rehabilitation measures applied to an existing building, or both. This code contains provisions for both a cyclic load test and a monotonic load test procedure.

Keywords: acceptance criteria; cyclic loading; load test; monotonic loading; test load magnitude; test protocol.

 

Document Details

Author: ACI Committee 437

Publication Year: 2014

ISBN: 9780870318917

Categories: Codes, Testing

Formats: PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—GENERAL

1.1—General

1.2—Scope

1.3—Purpose

1.4—Limitations

1.5—Interpretation

1.6—Language and units of measurement

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—REFERENCED STANDARDS

CHAPTER 4—TEST LOAD

4.1—Service loads

4.2—Test load magnitude

CHAPTER 5—LOADING PROTOCOL

5.1—Safety

5.2—Load arrangement

5.3—Monotonic loading protocol

5.4—Cyclic loading protocol

5.5—Load application

5.6—Response measurements

5.7—Visual inspection

CHAPTER 6—ACCEPTANCE CRITERIA

6.1—Distress caused by load test

6.2—Performance assessment at service load level

6.3—Acceptance criteria for monotonic loading protocol

6.4—Acceptance criteria for cyclic loading protocol

6.5—Provision for lower load rating

R7—COMMENTARY REFERENCES

Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).