364.3T-15 Treatment of Exposed Epoxy-Coated Reinforcement in Repair

364.3T-15 Treatment of Exposed Epoxy-Coated Reinforcement in Repair

Currency Choice

Your Price: $ 26.00 USD

Member Price: $ 21.00 USD

Save $ 5.00 USD, Become a Member

Choose Product Language

Choose Product Format


Description

This document outlines the treatment and repair of concrete areas containing epoxy-coated reinforcing steel when epoxy-coated reinforcing steel is exposed in a repair area.

Keywords:

coating; corrosion; corrosion inhibitor; electrical resistance; epoxy-coated; reinforcing bars; reinforcing steel; repair; ring anode effect; sacrificial anode.

 

Document Details

Author: ACI Committee 364

Publication Year: 2015

ISBN:

Categories: Repair

Formats: PDF

Table of Contents

Introduction

Answer

Discussion

Summary

References

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).