A review of published literature indicates that there is plenty of information regarding the pH of concrete as it relates to carbonation, embedded steel corrosion, alkali-silica reaction, and effects of mineral admixtures such as fly ash and silica fume. There are, however, only a few research papers published that are related to test methods to measure the pH of a concrete surface.

Portland cement and many other hydraulic-cement-based concretes are highly alkaline materials. Depending on the actual chemistry of the portland cement and amount of alkalis present, the pH of freshly placed concrete can vary from approximately 12 to over 13. The carbonation of concrete is known to lower the surface pH to a value in the vicinity of 9.

Keywords: adhesive compatibility; alkalinity; material properties; pH measurement; pH testing; resilient flooring adhesive; surface pH.

 

Document Details

Author: ACI Committee 364

Publication Year: 2018

Pages: 5.00

ISBN:

Categories: Repair

Formats: PDF

Table of Contents

Introduction

Question

Answer

Proposed method

Discussion

Summary

References

Authored documents

Appendix A

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).