362.1R-12 Guide for the Design and Construction of Durable Concrete Parking Structures

362.1R-12 Guide for the Design and Construction of Durable Concrete Parking Structures

Your Price: $65.50 USD

Member Price: $40.00 USD

Save $25.50 USD, Become a Member

Choose Product Language

Choose Product Format

Notes/Preview

Preview

Description

This guide presents design and construction criteria used to improve the durability of concrete parking structures. Emphasis is placed on key design criteria unique to parking structures, including structural systems, materials, structural design, durability, and construction. Also covered are cast-in-place nonprestressed concrete, cast-in-place post-tensioned concrete, and precast/prestressed concrete structural systems for use in parking structures.

Keywords: concrete durability; construction; corrosion; curing; finishes; freezing-and-thawing resistance; nonprestressed reinforcement; parking structures; post-tensioning; precast concrete; prestressed concrete.

Document Details

Author: ACI Committee 362

Publication Year: 2012

Pages: 24.00

ISBN: 9780870318009

Categories: Parking Structures

Formats: PDF, ePub, or Kindle

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Definitions

Chapter 3—Structural systems

3.1—General

3.2—Cast-in-place post-tensioned concrete systems

3.3—Cast-in-place reinforced (nonprestressed) concrete systems

3.4—Precast/prestressed concrete systems

3.5—Steel and concrete hybrid composite systems

3.6—Vehicle guardrail

3.7—Pedestrian guardrail

3.8—Below-grade parking structures

Chapter 4—Materials

4.1—General

4.2—Concrete

4.3—Nonprestressed reinforcement and reinforcement accessories

4.4—Prestressing

4.5—Embedded items

4.6—Surface treatments

4.7—Joint materials

Chapter 5—Structural design

5.1—Design criteria

5.2—Lateral-load-resisting systems

5.3—Vehicle barriers and guardrails

5.4—Deflection and camber

5.5—Restraint

5.6—Other design requirements

Chapter 6—Durability

6.1—General

6.2—Drainage

6.3—Design criteria tables

Chapter 7—Construction

7.1—General

7.2—Cast-in-place concrete construction

7.3—Precast concrete construction

7.4—Moisture protection

7.5—Quality control by contractor/quality assurance by owner

Chapter 8—References

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the Manual of Concrete Practice (MCP). For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).