355.3R-11 Guide for Design of Anchorage to Concrete: Examples Using ACI 318 Appendix D

Currency Display

Your Price:$ 123.50 USD

Member Price: $ 77.00 USD

Save $ 46.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

Description

This guide presents worked examples using the design provisions in ACI 318 Appendix D. Not all conditions are covered in these examples. The essentials of direct tension, direct shear, combined tension and shear, and the common situation of eccentric shear, as in a bracket or corbel, are presented.

Keywords: anchorage; combined tension and shear; design examples; eccentric shear; embedded bolts; headed-stud anchors; post-installed anchors; shear; tension.

 

Document Details

Author: ACI Committee 355

Publication Year: 2011

Pages: 124

ISBN: 9780870314254

Categories: Anchors

Formats: PDF or Protected PDF/Web View

This document is Historical

Table of Contents

Chapter 1—Introduction

1.1—Introduction

1.2—Discussion on design example problems

1.3—Commentary on seismic requirements for Appendix D of ACI 318-02 and ACI 318-05

1.4—Commentary on seismic requirements for Appendix D of ACI 318-08

1.5—Commentary on notation and definitions for Appendix D ACI 318-08

1.6—Anchor designs featured in example problems

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—ACI 318-05 Appendix D (reprinted)

Chapter 4—Design examples

4.1—Example 1: Single headed anchor away from edges subjected to seismic tension

4.2—Example 2: Single hooked anchor away from edges subjected to seismic tension

4.3—Example 3: Single post-installed anchor in tension away from edges

4.4—Example 4: Group of headed studs in tension near an edge

4.5—Example 5: Single headed bolt in shear near an edge

4.6—Example 6: Single headed bolt in tension and shear near an edge

4.7—Example 7: Single post-installed anchor in tension and shear near an edge

4.8—Example 8: Group of cast-in anchors in tension and shear with two free edges and supplemental reinforcement

4.9—Example 9: Group of headed studs in tension near an edge with eccentricity

4.10—Example 10: Multiple headed anchor connection subjected to moment and shear

4.11—Example 11: Multiple post-installed anchor connection subjected to seismic moment and shear

4.12—Example 12: Multiple headed anchor connection subjected to seismic moment and shear

4.13—Example 13: Group of tension anchors on a pier with shear lug

Chapter 5—References

5.1—Referenced standards and reports

5.2—Cited references

Appendix A—Tables

Table A.1—Materials for headed anchors and threaded rods

Table A.2(a)—Bearing area (Abrg) for cast-in anchors,threaded rod with nuts, and threaded rods

with nuts and washers

Table A.2(b)—Dimensional properties of bolts and studs for determining bearing area (Abrg)

Table A.2©—Dimensional properties of nuts for determining bearing area (Abrg)

Table A.3—Sample data for a post-installed, torquecontrolled mechanical expansion anchor

Table A.4—Sample data for a post-installed, undercut anchor

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.