Description
This specification covers minimum requirements for the construction of unreinforced concrete parking lots on grade. Included are requirements for submittals, testing and inspection, concrete materials, embedded reinforcement at joints, jointing and sealant material, forms, subgrade preparation, subbase, placing, texturing, curing, jointing, tolerances, and opening to traffic. This specification does not cover requirements for pervious concrete.
Keywords: construction; curing; inspection testing; jointing; pavements; site paving; texturing.
Table of Contents
PART 1—GENERAL
1.1—Scope
1.2—Definitions
1.3––Referenced standards
1.4—Submittals
1.5—Storage and handling
1.6—Testing and inspection
PART 2—PRODUCTS
2.1—Concrete
2.2—Embedded reinforcement at joints
2.3—Membrane-forming curing compounds
2.4—Joint and sealant material
2.5—Forms
PART 3—EXECUTION
3.1—Subgrade preparation
3.2—Subbase
3.3—Setting forms
3.4—Placing embedded reinforcement at joints
3.5—Batching, mixing, and delivery
3.6—Placing and finishing fixed-form pavement
3.7—Placing and finishing slipform and laser-guided
screed pavements
3.8—Edging
3.9—Final surface texture
3.10 Tolerances
3.11—Curing
3.12—Hot- or cold-weather construction
3.13—Jointing
3.14—Opening to traffic
NOTES TO SPECIFIER
General notes
(nonmandatory portion follows)
FOREWORD TO CHECKLISTS
MANDATORY REQUIREMENTS CHECKLIST
OPTIONAL REQUIREMENTS CHECKLIST
SUBMITTALS CHECKLIST
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).