325.9R-15 Guide for Construction of Concrete Pavements

325.9R-15 Guide for Construction of Concrete Pavements

Your Price: $ 102.50 USD

Member Price: $ 62.00 USD

Save $ 40.50 USD, Become a Member

Choose Product Language

Choose Product Format

Notes/Preview

Preview

Description

The primary focus of this guide is pavement construction. Modern slipform paving techniques and time-proven formed construction procedures are highlighted. Quality control, quality assurance, and construction inspection, as well as the environmental, economic, and societal benefits of concrete pavement, are also presented.

This guide briefly reviews all aspects of concrete pavement construction for highways and, to some extent, local roads, streets, and airfields. Intended for field and office personnel, this guide provides a background on design issues that relate to construction and reviews material selection.

Note that the materials, processes, quality control measures, and inspections described in this guide should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certifications or equivalent.

Keywords: concrete pavement; concrete pavement construction; concrete paving; fixed-form paving; paving materials; slipform paving; sustainability.

 

Document Details

Author: ACI Committee 325

Publication Year: 2015

Pages: 62.00

ISBN: 9781942727316

Categories: Pavements

Formats: Printed Document, PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—ACRONYMS AND DEFINITIONS

2.1—Acronyms

2.2—Definitions

CHAPTER 3—DESIGN ISSUES RELATING TO CONSTRUCTION

3.1—Introduction

3.2—Design principles

3.3—Current design procedures

3.4—Critical design inputs for construction

3.5—Pavement design considerations

3.6—City streets

3.7—Drainage issues

CHAPTER 4—MATERIAL SELECTION

4.1—Introduction

4.2—Foundation materials

4.3—Pavement concrete materials

4.4—Reinforcement, dowels, and tie bars

4.5—Joint sealants and fillers

4.6—Curing materials

CHAPTER 5—CONSTRUCTION

5.1—Foundation preparation

5.2—Production, placing, consolidation, and finishing concrete pavement

5.3—Curing and enhancing characteristics of concrete

5.4—Installation of joints and reinforcement

5.5—Dowels and tie bars

5.6—Placing embedded reinforcement

5.7—Texturing

5.8—Tolerances

5.9—Extreme weather conditions

5.10—Opening to traffic

5.11—Quality control/quality assurance

5.12—Construction inspection

CHAPTER 6—SUSTAINABILITY

6.1—Introduction

6.2—Sustainable concrete pavements

6.3—Societal benefits of concrete pavement

6.4—Environmental benefits of concrete pavement

6.5—Economic benefits of concrete pavement

6.6—Conclusion

CHAPTER 7—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).