ACI PRC-325.12-26: Design of Jointed Concrete Pavements for Streets and Local Roads—Guide

ACI PRC-325.12-26: Design of Jointed Concrete Pavements for Streets and Local Roads—Guide

Price: $ 54.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Description

This guide provides a perspective on a balanced combination of pavement thickness, drainage, and subbase or subgrade materials to achieve an acceptable pavement system for streets and local roads. Such concrete pavements designed for low volumes of traffic—typically less than 100 trucks per day, one-way—have historically provided satisfactory performance when proper support and drainage conditions exist. Recommendations are presented for designing a concrete pavement system for a low volume of traffic and associated joint pattern based upon limiting the stresses in the concrete or, in the case of reinforced slabs, maintaining the cracks in a tightly closed condition. Details for designing the distributed reinforcing steel and the load transfer devices are given, if required.

The thickness design of low-volume concrete pavements is based on the principles developed by the American Cement Association and others for analyzing an elastic slab over a dense liquid subgrade, as modified by field observations and extended to include fatigue concepts.

Keywords:

dowel; flexural strength; joint; pavement; portland cement; quality control; slipform; subbase; tie bar.

 

Document Details

Author: ACI Committee 325

Publication Year: 2026

Pages: 48

ISBN: 9781641953672

Categories: Pavements

Formats: Printed Document or Protected PDF/Web View

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE, p. 2

1.1—Introduction, p. 2

1.2—Scope, p. 2

1.3—Background, p. 2

CHAPTER 2—DEFINITIONS, p. 3

2.1—Definitions, p. 3

CHAPTER 3—PAVEMENT MATERIAL REQUIREMENTS, p. 4

3.1—Support conditions, p. 4

3.2—Properties of concrete paving mixtures, p. 7

CHAPTER 4—PAVEMENT THICKNESS DESIGN, p. 9

4.1—Basis of design, p. 9

4.2—Traffic, p. 9

4.3—Thickness determination, p. 10

4.4—Economic factors, p. 13

4.5—Environmental factors, p. 14

4.6—Life-cycle assessment, p. 14

CHAPTER 5—PAVEMENT JOINTING, p. 14

5.1—Slab length and related design factors, p. 15

5.2—Transverse joints, p. 17

5.3—Longitudinal joints, p. 19

5.4—Isolation joints, p. 20

5.5—Slab reinforcement, p. 21

5.6—Irregular panels, p. 21

5.7—Contraction joint sealants, p. 21

CHAPTER 6—SUMMARY, p. 24

CHAPTER 7—REFERENCES, p. 24

Authored documents, p. 26

APPENDIX A—PAVEMENT THICKNESS DESIGN CONCEPTS, p. 28

A.1—Load stresses and fatigue calculations, p. 28

A.2—Proprietary design software, p. 30

A.3—Joint spacing method, p. 30

APPENDIX B—SUBGRADE, p. 31

B.1—Introduction, p. 31

B.2—Soil classification, p. 31

B.3—Geotechnical investigations, p. 31

B.4—Expansive soils, p. 34

B.5—Frost action, p. 35

B.6—Pumping, p. 36

APPENDIX C—JOINTING DETAILS FOR PAVEMENTS AND APPURTENANCES, p. 36

APPENDIX D—PAVEMENT MAINTENANCE AND REHABILITATION, p. 40

D.1—Surface sealing, p. 41

D.2—Joint resealing and crack sealing, p. 41

D.3—Partial-depth repair, p. 41

D.4—Full-depth repair, p. 42

D.5—Undersealing and leveling, p. 42

D.6—Overlays, p. 42

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).