325.11R-01: Accelerated Techniques for Concrete Paving

325.11R-01: Accelerated Techniques for Concrete Paving

Currency Display

Your Price: $ 41.50 USD

Member Price: $ 25.00 USD

Save $ 16.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This report covers the state of the art of accelerated-concrete paving techniques, often referred to as "fast-track" concrete paving. Accelerated-concrete paving techniques are appropriate for roadways, airfield, and other paved surfaces where quick access is required. Considerations include planning, concrete materials and properties, jointing and joint sealing, curing and temperature control, concrete strength testing, and opening-to-traffic criteria. Applications and uses of accelerated-concrete paving are discussed.

Keywords: accelerated paving; airports; admixtures; aggregates; cement; construction; concrete pavement; curing; fast-track paving; gradation; highways; intersections; joint sealing compound; jointing; nondestructive strength testing; specifications; streets; temperature; opening-to-traffic.

 

Document Details

Author: ACI Committee 325

Publication Year: 2002

Pages: 18

ISBN: 9780870310232

Categories: Pavements

Formats: PDF

This document is Historical

Table of Contents

Chapter 1--Introduction

1.1--General

1.2--Changes to construction specifications and processes

Chapter 2--Project applications

2.1--General

2.2--Highways and tollways

2.3--Streets

2.4--Intersections

2.5--Airports

Chapter 3--Planning

3.1--Planning considerations

3.2--Lane rental

3.3--Partnering

3.4--Specifications

3.5--Innovative equipment

Chapter 4--Concrete materials

4.1--Concrete mixute proportioning

4.2--Cement

4.3--Supplementary cementitious materials

4.4--Air-entraining admixture

4.5--Water-reducing admixtures

4.6--Accelerating admixtures

4.7--Aggregate

4.8--Water

Chapter 5--Construction

5.1--General

5.2--Curing and temperature management

5.3--Jointing and sealing

Chapter 6--Nondestructive testing

6.1--Appropriate methods

6.2--Maturity

6.3--Pulse-velocity

Chapter 7--Traffic opening

7.1--Strength criteria

7.2--Construction traffic

7.3--Public traffic

7.4--Aircraft traffic

Chapter 8--References

8.1--Referenced standards and reports

8.2--Cited references

8.3--Other references

Appendix--Opening to public traffic

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.