This guide reviews and describes practices, procedures, materials, and monitoring methods for the external curing of concrete and provides guidance for specifying curing procedures. Current curing techniques are presented and commonly accepted methods, procedures, and materials are described. Methods are given for curing structures and buildings, pavements and other slabs-on-ground, and for mass concrete. Curing methods for several specific categories of cement-based products are discussed in this document.

The materials, processes, quality control measures, and inspections described in this document should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI certifications or equivalent.

Keywords: cold weather construction; curing compound; hot weather construction; mass concrete; reinforced concrete; sealer; shotcrete; slabs-on-ground.

 

Document Details

Author: ACI Committee 308

Publication Year: 2016

Pages: 36

ISBN: 9781942727873

Categories: Curing

Formats: Printed Document, Protected PDF/Web View, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION

1.1—Introduction

1.2—Curing

1.3—Curing and hydration of portland cement

1.4—Deliberate curing procedures

1.5—Curing-affected zone

1.6—Concrete properties influenced by curing

1.7—Effects of elevated temperature

1.8—Sustainability

CHAPTER 2—DEFINITIONS

CHAPTER 3—CURING METHODS AND MATERIALS

3.1—Scope

3.2—Use of water for curing concrete

3.3—Initial curing methods

3.4—Final curing measures

3.5—Termination of curing measures

3.6—Cold-weather protection and curing

3.7—Hot-weather protection and curing

3.8—Accelerated curing

3.9—Minimum curing requirements

3.10—Temperature limits during curing

CHAPTER 4—CURING FOR DIFFERENT TYPES OF CONSTRUCTION

4.1—Pavements and other slabs on ground

4.2—Buildings, bridges, and other structures

4.3—Mass concrete

4.4—Curing colored concrete floors and slabs

4.5—Specialty constructions

CHAPTER 5—MONITORING CURING AND CURING EFFECTIVENESS

5.1—General

5.2—Evaluating environmental conditions

5.3—Means to verify application of curing

5.4—Impact of curing procedures on immediate environment

5.5—Impact of curing procedures on moisture and temperature within concrete

5.6—Maturity method

5.7—Assessing curing effectiveness

CHAPTER 6—REFERENCES

Authored references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.