This report presents technical information to support the use of high-volume fly ash concrete for structural applications. The advantages and limitations of high volume fly ash concrete are discussed, and the characteristics of the fresh and hardened materials and the durability of the material to various aggressive environments are covered. Field applications are presented along with sustainability features.

Keywords: alkali-silica reaction; compressive strength; corrosion of reinforcement; cracking; deicing salts; fly ash; heat of hydration; mixture proportions; modulus of elasticity; shrinkage; sulfate attack; sustainability; tensile strength.

 

Document Details

Author: ACI Committee 232

Publication Year: 2014

Pages: 19.00

ISBN: 9780870319464

Categories: Fly Ash

Formats: Printed Document or PDF

Table of Contents

CHAPTER 1—GENERAL

1.1—Introduction

1.2—Significance

1.3—Historical backgrond

1.4—Sustainability

1.5—Classification of HVFA concrete

1.6—Types of fly ash and portland cement

1.7—Codes and specifications

1.8—In-place strength

CHAPTER 2—DEFINITIONS

CHAPTER 3—CHARACTERISTICS OF FRESH HVFA CONCRETE

3.1—Materials and mixture proportions

3.2—Slump and workability

3.3—Setting time

3.4—Heat of hydration

3.5—Plastic shrinkage cracks

CHAPTER 4—CHARACTERISTICS OF HARDENED HVFA CONCRETE

4.1—Compressive strength

4.2—Tensile strength

4.3—Modulus of elasticity

4.4—Shrinkage and creep

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).