231R-10 Report on Early-Age Cracking: Causes, Measurement and Mitigation

231R-10 Report on Early-Age Cracking: Causes, Measurement and Mitigation

Your Price: $ 76.50 USD

Member Price: $ 46.00 USD

Save $ 30.50 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

Preview

Description

Early-age cracking is a challenge for the concrete industry. Materials selection, environmental conditions, and field practices all have considerable influence on the propensity for early-age cracking to occur. This document focuses on thermal- and moisture-related deformations; both are materials-related and contribute to early-age cracking. The document provides detailed reviews on the causes of deformation and cracking, test methods for assessing shrinkage and thermal deformation properties, and mitigation strategies for reducing early-age cracking.

Keywords: autogenous shrinkage; cracking; early-age; heat of hydration; measurement; mitigation methods; microstructure; shrinkage; shrinkage cracking; sustainability; thermal cracking; thermal properties.

 

Document Details

Author: ACI Committee 231

Publication Year: 2010

Pages: 46.00

ISBN: 9780870313592

Categories: Cracking

Formats: PDF

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Causes of early-age deformation and cracking

3.1—Thermal deformation

3.2—Autogenous shrinkage

3.3—Drying shrinkage

3.4—Creep and stress relaxation from deformation restraint

3.5—Mitigation of shrinkage

Chapter 4—Test methods and assessment

4.1—Introduction

4.2—Shrinkage measurements

4.3—Ring test

4.4—Rigid cracking frames

4.5—Coefficient of thermal expansion (αT) measurement

4.6—Analysis tools assessing stresses and cracking

Chapter 5—Shrinkage control

5.1—Introduction

5.2—Expansive additives

5.3—Shrinkage-reducing admixtures

5.4—Internal curing

Chapter 6—References

6.1—Referenced standards and reports

6.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).