224.2R-92: Cracking of Concrete Members in Direct Tension (Reapproved 2004)

224.2R-92: Cracking of Concrete Members in Direct Tension (Reapproved 2004)

Your Price: $ 25.50 USD

Member Price: $ 16.00 USD

Save $ 9.50 USD, Become a Member

Choose Product Language

Choose Product Format


Description

This report is concerned with cracking in reinforced concrete caused primarily by direct tension rather than bending. Causes of direct tension cracking are reviewed, and equations for predicting crack spacing and crack width are presented. As cracking progresses with increasing load, axial stiffness decreases. Methods for estimating postcracking axial stiffness are discussed. The report concludes with a review of methods for controlling cracking caused by direct tension.

Keywords: cracking (fracturing); crack width and spacing; loads (forces); reinforced concrete; restraints; stiffness; strains; stresses; tensile stress; tension; volume change.

 

Document Details

Author: ACI Committee 224

Publication Year: 2002

Pages: 12.00

ISBN: 9780870310355

Categories: Cracking

Formats: PDF

Table of Contents

Chapter 1: Introduction

Chapter 2: Causes of cracking

* Introduction

* Applied loads

* Restraint

Chapter 3: Crack behavior and prediction equations

* Introduction

* Tensile strength

* Development of cracks

* Crack spacing

* Crack width

Chapter 4: Effect of cracking on axial stiffness

* Axial stiffness of one-dimensional members

* Finite element applications

* Summary

Chapter 5: Control of cracking caused by direct tension

* Introduction

* Control of carcking caused by applied loads

* Control of cracking caused by restraint of volume change

Notation

Conversion Factors

Chapter 6: References

* Recommended references

* Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).