Description

This guide describes adjustments that can be made to existing proportions for normal-density concrete with and without chemical admixtures, pozzolans, and slag. These adjustments are based on the performance of the concrete mixture as used in construction. The adjustments consider evaluation for placeability, consistency, strength, and durability. The procedures used in making these adjustments can be found in ACI 211.1. Adjustments to concrete mixture proportions or sources may require resubmittal to the design professional as detailed in ACI 301. This guide also provides information regarding jobsite conditions and testing practices that should be evaluated before adjustments are made to the mixture.

Keywords: admixtures; aggregates; cementitious materials; durability; fine aggregates; fly ash; metakaolin; mixture proportioning; pozzolans; quality; silica fume; slag; slag cement; slump tests; water-cementitious material ratio.

 

Document Details

Author: ACI Committee 211

Publication Year: 2015

Pages: 9.00

ISBN: 9781942727262

Categories: Mixture Proportioning

Formats: Printed Document, PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—DEFINITIONS

CHAPTER 3—REASONS FOR ADJUSTING MIXTURE PROPORTIONS

CHAPTER 4—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).