211.4R-08: Guide for Selecting Proportions for High-Strength Concrete Using Portland Cmt & Other Cementitious Material

211.4R-08: Guide for Selecting Proportions for High-Strength Concrete Using Portland Cmt & Other Cementitious Material

Your Price: $ 55.50 USD

Member Price: $ 34.00 USD

Save $ 21.50 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

Preview

Description

This guide presents general methods for selecting mixture proportions forhigh-strength concrete and optimizing these mixture proportions on thebasis of trial batches. The methods are limited to high-strength concrete containing portland cement and fly ash, silica fume, or slag cement(formerly referenced as ground-granulated blast-furnace slag) andproduced using conventional materials and production techniques.Recommendations and tables are based on current practice and infor-mation provided by contractors, concrete suppliers, and engineers whohave been involved in projects dealing with high-strength concrete.

Keywords: aggregate; fly ash; high-range water-reducing admixture; high-strength concrete; mixture proportion; quality control.

 

Document Details

Author: ACI Committee 211

Publication Year: 2009

Pages: 25.00

ISBN: 9780870313141

Categories: Mixture Proportioning

Formats: PDF

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Performance requirements

3.1—Test age

3.2—Required average compressive strength for f ' cr

3.3—Other requirements

Chapter 4—Concrete materials

4.1—Introduction

4.2—Portland cement

4.3—Fly ash

4.4—Silica fume

4.5—Slag cement

4.6—Combinations of other cementitious materials

4.7—Mixing water

4.8—Coarse aggregate

4.9—Fine aggregate

4.10—Chemical admixtures

Chapter 5—High-strength concrete mixture properties

5.1—Introduction

5.2—Water-cementitious material ratio

5.3—Workability

Chapter 6—High-strength concrete mixture proportioning using fly ash

6.1—Fundamental relationship

6.2—Concrete mixture proportioning

6.3—Sample calculations

Chapter 7—High-strength concrete mixture proportioning using silica fume

7.1—Fundamental relationships

7.2—Concrete mixture proportioning

7.3—Sample calculations

Chapter 8—High-strength concrete mixture proportioning using slag cement

8.1—Fundamental relationships

8.2—Concrete mixture proportioning

8.3—Sample calculations

Chapter 9—References

9.1— Referenced standards and reports

9.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).