211.3R-02: Guide for Selecting Proportions for No-Slump Concrete (Reapproved 2009)

211.3R-02: Guide for Selecting Proportions for No-Slump Concrete (Reapproved 2009)

Your Price: $58.50 USD

Member Price: $34.00 USD

Save $24.50 USD, Become a Member

Choose Product Language

Choose Product Format


Description

Intended as a suuplement to "Standard Practice for Selecting Proportions for Normal, Heavyweight and Mass Concrete" (ACI 211.1). The standard describes a procedure for proportioning concretes having slumps in the range of zero to 3 inch and consistencies below this range, for aggregates up to 1 inch maximum size. Suitable equipment for measuring such consistencies is described. Tables similar to those in ACI 211.1 are provided which, along with laboratory tests on physical properties of fine and coarse aggregate, yield information for obtaining concrete proportions for a trial mixture. Examples of the use of these tables are given. An appendix provides complete conversion of all tabular data to metric system units and shows a sample problem worked out with metric values.

Keywords: durability; mixture proportioning; no-slump concrete; rollercompacted

concrete; slump test; water-cementitious materials ratio.

 

Document Details

Author: ACI Committee 211

Publication Year: 2002

Pages: 26.00

ISBN: 9780870310775

Categories: Mixture Proportioning

Formats: PDF

This document is Withdrawn

Table of Contents

Chapter 1 -- Scope and limits

Chapter 2 -- Preliminary considerations

2.1 -- General

2.2 -- Methods for measuring consistency

2.3 -- Mixing water requirement

Chapter 3 -- Selecting Proportions

3.1 -- General

3.2 -- Slump and miximum size of aggregate

3.3 -- Estimating water requirements

3.4 -- Selecting water-cement ratio

3.5 -- Estimate of quantity of coarse aggregate

Chapter 4 -- Computation of proportions

4.1 -- General design criteria

4.2 -- Example of computation of proportions

4.3 -- Batch weights for field use

4.4 -- Adjustment of trial mixture

References

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).