207.4R-05: Cooling and Insulating Systems for Mass Concrete (Reapproved 2012)

207.4R-05: Cooling and Insulating Systems for Mass Concrete (Reapproved 2012)

Your Price: $47.50 USD

Member Price: $28.00 USD

Save $19.50 USD, Become a Member

Choose Product Language

Choose Product Format


Notes/Preview

Click here to preview

Description

The need to control volume change induced primarily by temperature change in mass concrete often requires cooling and insulating systems. This report reviews precooling, postcooling, and insulating systems. A simplified method for computing the temperature of freshly mixed concrete cooled by various systems is also presented.

Keywords: cement content; coarse aggregate; creep; formwork; heat of

hydration; mass concrete; modulus of elasticity; precooling; postcooling;

pozzolan; restraint; specific heat; strain; stress; temperature rise; tensile

strength; thermal conductivity; thermal diffusivity; thermal expansion; thermal

gradient; thermal shock.

Document Details

Author: ACI Committee 207

Publication Year: 2005

Pages: 15.00

ISBN: 9780870311918

Categories: Mass Concrete

Formats: PDF

Table of Contents

Chapter 1—Introduction

1.1—Scope and objective

1.2—Historical background

1.3—Types of structures and temperature controls

1.4—Construction practices for temperature control

1.5—Instrumentation

Chapter 2—Precooling systems

2.1—General

2.2—Heat exchange

2.3—Batch water

2.4—Aggregate cooling

2.5—Cementitious materials

2.6—Heat gains during concreting operations

2.7—Refrigeration plant capacity

2.8—Placement area

Chapter 3—Postcooling systems

3.1—General

3.2—Embedded pipe

3.3—Refrigeration and pumping facilities

3.4—Operational flow control

3.5—Surface cooling

Chapter 4—Surface insulation

4.1—General

4.2—Materials

4.3—Horizontal surfaces

4.4—Formed surfaces

4.5—Edges and corners

4.6—Heat absorption from light energy penetration

4.7—Geographical requirements

Chapter 5—References

5.1—Referenced standards and reports

5.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the Manual of Concrete Practice (MCP). For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).