Title: Letter Perfect

Author(s): William E. Schwarz

Publication: Concrete International

Volume: 8

Issue: 10

Appears on pages(s): 32-33

Keywords:

Date: 10/1/1986

Abstract:
Letters are delicate things-even when they ar made from concrete. So repairing the letters that spell out the name Portland Cement Association on the face of PCA's research and development building was a tricky job.