Standard Practice for the Inspection of Concrete

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Standard Practice for the Inspection of Concrete

Author(s): Roger E. Wilson

Publication: Concrete International

Volume: 4

Issue: 9

Appears on pages(s): 55-57

Keywords: acceptability; aggregates; concrete con-struction; contractors; inspection; quality control; ready-mixed concrete; testing laboratories; tests.

Date: 9/1/1982

Abstract:
ACI Committee 311 is in the process of writing a Standard Practice for the Inspection of Concrete. It is to include quality control (product control) inspection by the contractor or subcontractor, and acceptance inspection by the owner or his representative. An Initial outline has been prepared and is being addressed by position papers.