In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: Climbing Formwork Captures the European Market
Author(s): Ernst Roeck
Publication: Concrete International
Volume: 4
Issue: 6
Appears on pages(s): 33-37
Keywords: concrete construction; cranes (hoists); formwork (construction); reinforced concrete; slip-form construction.
Date: 6/1/1982
Abstract:Describes the development of this method in Europe, explaining the main differences between slip-forming and climbing formwork and the latter’s specific advantages. Examples are given both for sites using climbing and self-climbing formwork.