Title: Lining of the Alva B. Adams Tunnel

Author(s): Richrard J. Willson

Publication: Journal Proceedings

Volume: 43

Issue: 11

Appears on pages(s): 209-238

Keywords: none

Date: 11/1/1946

Abstract:
The 13.03 mile Alva B. Adams Tunnel, excavated under the Continental Divide, as a part of the trans mountain water diversion plan of the Colorado-Big Thompson Project, United States Department of the Interior, Bureau of Reclamation, is lined with concrete. Lining equipment and methods and aggregate processing are described.