In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: The Physical Properties Of Cast Stone
Author(s): John Tucker, JR., G. W. Walker and J. Arthur
Publication: Journal Proceedings
Volume: 28
Issue: 12
Appears on pages(s): 243-264
Keywords: none
Date: 12/1/1931
Abstract:A report of results of tests made as basis from which the Federal S ecification for Cast Stone was prepared. The 68 samp es were representative of all the usual methods of fabrication and included a wide variety of aggregate. The strengths, absorption properties, and resistance to freezing and thawing were determined. The compressive strengths varied from I558 to 21,720 the 48-hr absorption from 2.0 to 13.1 percent. Resistance to freezing and thawing varied from complete disintegration at 25 cycles to the first signs of disintegration at 1450 cycles.