Title: Concrete Plant On Detroit Water Filtration Substructure

Author(s): W. K. Saunders

Publication: Journal Proceedings

Volume: 28

Issue: 10

Appears on pages(s): 97-108

Keywords: none

Date: 10/1/1931

Abstract:
To handle and deposit approximately 75,008 cu yd of concrete over an area about 600 sq ft, several methods of placing were considered. Belt conve ors offered a flexible system and were used successfu ly. R




  