Title: Design and Operation Of Central Mixing Plants

Author(s): Frank I. Ginsberg

Publication: Journal Proceedings

Volume: 27

Issue: 6

Appears on pages(s): 1237-1249

Keywords: none

DOI: 10.14359/8224

Date: 6/1/1931

Abstract:
Outlines the progress in central plant design and operation. The conditions that govern the design and arrangement of ready-mixed concrete plants are controlled by a number of local factors. The items covered include: types of plants, equipment methods, handling of bulk cement, and types of trucks used delivery.




  