Title: Australian Experiments With Flat Plates

Author(s): Frank A. Blakey

Publication: Journal Proceedings

Volume: 60

Issue: 4

Appears on pages(s): 515-526

Keywords:

Date: 4/1/1963

Abstract:
Describes three experimental flat plate structures erected and tested by the Commonwealth Scientific and Industrial Research Organization , Australia. Some of the more interesting results of the tests are presented.




  