Title: Behavior of Plain Concrete Under Axial Tension
Author(s): Vedat A. Yerlici
Publication: Journal Proceedings
Volume: 62
Issue: 8
Appears on pages(s): 987-992
Keywords: creep, plain concrete, research, tensile load, tensile, strength
Date: 8/1/1965
Abstract:
The strength and extension of plain concrete under short-time, repeated, and sustained axial tensile load are discussed. Formulas are given to approximate instantaneous and time dependent strain of concrete under constant or variable tensile stress