Title: A General Relation for Strengths of Concrete Specimens of Different Shapes and Sizes

Author(s): Adam M. Neville

Publication: Journal Proceedings

Volume: 63

Issue: 10

Appears on pages(s): 1095-1110

Keywords: compression tests, compressive strength, concrete, correlation, cubes, cylinders, fineness modulus, prisms.

Date: 10/1/1966

Abstract:
It is shown that the strengths of concrete test specimens(cylinders, cubes, and prisms) can be related to one another by simple expressions. Substantiating test results are pre-sented. The secondary influence of the fineness modulus of aggregate on this relation is discussed.