Title: Computer Graphics Applications

Author(s): ACI Committee 118

Publication: Journal Proceedings

Volume: 68

Issue: 11

Appears on pages(s): 813-824

Keywords: Architecture, civil engineering, computer programs, gaphic methods, reinforced concrete, structural design

Date: 11/1/1971

Abstract:
Examines state of art, applications in survey of over 100 engineering organizations using computer graphics.