Terminal Road Bridges for San Francisco International Airport Airport,”

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Terminal Road Bridges for San Francisco International Airport Airport,”

Author(s): Y.C. Yang

Publication: Journal Proceedings

Volume: 69

Issue: 10

Appears on pages(s): 614-618

Keywords: Airports, architectural concrete, bridges (structures), concrete construction, con-struction costs, prestressed concrete, re-inforced concrete, structural design

Date: 10/1/1972

Abstract:
Planning, design and construction of two parallel elevated road bridges for San Francisco International Airport expansion described. Design utilized precast, prestressed inverter double-T panels, cantilevering 22 feet each side from central spinal beam.