Title: Measurement of Thickness of Concrete Pavement and Structural Members

Author(s): Toshiaki Takabayashi and Hiroshi lshida

Publication: Special Publication

Volume: 82

Issue:

Appears on pages(s): 659-672

Keywords: concrete pavements; nondestructive tests; resonant frequency; thickness; ultrasonic tests.

Date: 9/1/1984

Abstract:
This paper describes a method of measuring the thickness of pavement concrete and other concrete structural members. A particular feature of this method involves the combined usage of the ultra-sonic pulse and resonance methods to compute the thickness of concrete by measuring the sonic velocity and resonance frequency of concrete.