Title: Thermal Stresses in Square Shaped Concrete Pavements

Author(s): J. Silfwerbrand

Publication: Symposium Paper

Volume: 181

Issue:

Appears on pages(s): 1-16

Keywords: Concrete pavements; square slabs; thermal stresses

Date: 3/1/1999

Abstract:
Thermal stresses in concrete pavements might be calculated according to a procedure developed by professor J. Eisenmann. The thermal stresses are dependent on the subgrade stiffness. Soft subgrades result in lower stresses. The Eisenmann procedure has been developed to cover square shaped slabs. This procedure is presented and discussed. in this paper. Two calculation examples are also presented




  