Title: E3-83: Hydraulic Cement for Concrete
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 36
Keywords: cement
Date: 7/1/1983
Abstract:
Note: A newer version of this document exists. This document was replaced by E3-01.
An ACI Education Bulletin presents a fundamental discussion on the manufacture, properties, characteristics, and specifications for portland cements. Topics include types of cements, tests for cement, and factors in selection and use of portland cement.