ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: 318-95/318-95: Building Code Requirements for Structural Concrete & Commentary

Author(s): ACI Committee 318

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 370

Keywords:

DOI:

Date: 7/1/1995

Abstract:
Note: A newer version of this document exists. This document was replaced by 318-99. The code portion of this document covers the proper design and construction of buildings of structural concrete. The code has been written in such form that it may be adopted by reference in a general building code and earlier editions have been widely used in this manner. Among the subjects covered are: drawings and specifications; inspection; materials; durability requirements; concrete quality, mixing, and placing; formwork; embedded pipes and construction joints; reinforcement details; analysis and design; strength and serviceability; flexural and axial loads; shear and torsion; development and splices of reinforcement; slab systems; walls; footings; precast concrete; composite flexural members; prestressed concrete; shells and folded plate members; strength evaluation of existing structures; special provisions for seismic design; structural plain concrete; an alternate design method in Appendix A; unified design provisions in Appendix B; and alternative load and strength reduction factors in Appendix C. The quality and testing of materials used in the construction are covered by reference to the appropriate ASTM standard specifications. Welding of reinforcement is covered by reference to the appropriate ANSI/AWS standard.