ENSAYOS SOBRE UN TIPO ESPECIAL DE UNION VIGA-LOSA PARA PUENTES O VIADUCTOS DE HORMIGON PRETENSADO.

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: ENSAYOS SOBRE UN TIPO ESPECIAL DE UNION VIGA-LOSA PARA PUENTES O VIADUCTOS DE HORMIGON PRETENSADO.

Author(s): Matera, E.

Publication: ACHE

Volume: 24

Issue: 106

Appears on pages(s): 67 -

Keywords: 0

Date: 1/1/1973

Abstract: