CRC 88: Proposed Specification for Deformed Steel Bars with Controlled Ductile Properties for Concrete Reinforcement

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: CRC 88: Proposed Specification for Deformed Steel Bars with Controlled Ductile Properties for Concrete Reinforcement

Author(s): Wiss, Janney, Elstner Associates, Inc.

Publication: CRC

Volume:

Issue:

Appears on pages(s):

Keywords:

Date: 7/10/2015

Abstract:
As requested by the Charles Pankow Foundation (CPF), Wiss, Janney, Elstner Associates, Inc. (WJE) has developed a draft of a proposed manufacturing specification for deformed steel reinforcing bars with controlled ductile properties having specified minimum yield strengths of up to 100,000 psi (690 MPa). The development of the proposed specification was carried out as a part of CPF RGA #03-14, which was awarded to WJE on June 2, 2014 and subsequently amended on October 14, 2014. This research effort is in support of CPF's research project in the area of High Strength Steel Bar Reinforcement (High Strength Rebar).