Title: Experimental Study on the Shear Behavior of RC Beams with Corroded Stirrups

Author(s): Shanhua Xu, Zongxing Zhang, Rou Li, Bin Qiu

Publication: JCI

Volume: 15

Issue: 4

Appears on pages(s): 178 - 189

Keywords:

Date: 1/1/2017

Abstract: