Title: Evaluation of Damage in Concrete Suffered Freeze-Thaw Cycles by CT Technique

Author(s): Wei Tian, Nv Han

Publication: JCI

Volume: 14

Issue: 11

Appears on pages(s): 679 - 690

Keywords:

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access.