Title: Modeling of Corrosion-Induced Damage in Reinforced Concrete Considering Electro-Mechanical Coupling

Author(s): Di Qiao, Hikaru Nakamura, Yoshihito Yamamoto, Taito Miura

Publication: JCI

Volume: 14

Issue: 11

Appears on pages(s): 664 - 678

Keywords:

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access.

View Resource »