Title: Residual Static Strength of Concrete Cylinder Specimen and Stud Anchor Specimen after Cyclic Loadings

Author(s): Osamu Kontani, Naoki Ishitobi, Junya Kawada, Noriaki Taogoshi, Makoto Koge, Yoshito Umeki

Publication: JCI

Volume: 14

Issue: 10

Appears on pages(s): 634 - 642

Keywords:

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access.