Title: Influence of Temperature and Added Lime on the Glassy Phase Dissolution in Low-calcium Fly ash Binary Blend

Author(s): Gangapatnam. V. P. Bhagath Singh, Kolluru V. L. Subramaniam

Publication: JCI

Volume: 14

Issue: 9

Appears on pages(s): 614 - 624

Keywords:

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access.