Title: Effects of Electrochemical Chloride Extraction on Hydrated Products of Various Cement Paste Systems

Author(s): Hai Yen Nguyen Thi, Hiroshi Yokota, Katsufumi Hashimoto

Publication: JCI

Volume: 13

Issue: 12

Appears on pages(s): 564 - 582

Keywords:

Date: 1/1/2015