Title: Fire Resistance of Reinforced Concrete Frames Subjected to Service Load: Part 1. Experimental Study

Author(s): Mohammad Mahdi Raouffard, Minehiro Nishiyama

Publication: JCI

Volume: 13

Issue: 12

Appears on pages(s): 554 - 563

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.