Title: Effect of the Mineral Admixtures on Pipe Flow of Pumped Concrete

Author(s): Myoung Sung Choi, Sung Bum Park, Su-Tae Kang

Publication: JCI

Volume: 13

Issue: 11

Appears on pages(s): 489 - 499