Title: Scale Effect on CFRP Strengthening of Infilled Reinforced Concrete Frames

Author(s): Emre Akın, Erdem Canbay, Barış Binici, Güney Özcebe

Publication: JCI

Volume: 13

Issue: 7

Appears on pages(s): 355 - 366

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.