Title: Modeling of High-Strength FRC Structural Elements with Spatially Non-Uniform Fiber Volume Fraction

Author(s): Petr Kabele, Tereza Sajdlová, Milan Rydval, Jiří Kolísko

Publication: JCI

Volume: 13

Issue: 6

Appears on pages(s): 311 - 324

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.