Title: Theoretical and Experimental Investigation of Loading Effects on Chloride Diffusion in Saturated Concrete

Author(s): Chuanqing Fu, Xianyu Jin, Hailong Ye, Nanguo Jin

Publication: JCI

Volume: 13

Issue: 1

Appears on pages(s): 30 - 43

Keywords:

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access.